Mô tả
Printing speed | 2-4 seconds | |
Critical exposure energy | 6-13mJ/ cm³ | 405nm |
Curing depth | 0.015-0.08mm | 405nm |
Shrinkage rate | ≤1.5% | |
Hardness shore D | 80D | |
Flexural modulus | 3000 | |
Strength at break | 60MPa | |
Stretching rate | 10% | |
Hot deformation temperature | 100 ℃ |